Part 5 · Design for printing

Joints & fasteners

Snap-fits that survive more than one use, nut traps that actually hold a nut, heat-set inserts, magnets, hinges, gears and every other way to hold printed parts together, with the dimensions that work on a 0.4 mm nozzle.

Intermediate⏱ 50 min read
What you will learn

How to choose between a snap-fit, a screw, an insert, a magnet and glue; how to size a cantilever snap-fit with simple beam math and a strain limit for your material; the pocket dimensions for M2–M8 nuts, heads and heat-set inserts; and the details that make hinges, bearings, gears and split parts go together. Clearances come from Tolerances & fits; strength reasoning from Strength & orientation. Complete mechanisms built from these joints (hinges, latches, mounts, slides, clamps) are compared in the Mechanism catalog.

🔰 Choosing a joint

Every joint is a trade between strength, reusability, assembly effort and extra hardware. Printing gives you geometry for free, so the cheapest joint is often one that needs no hardware at all (a snap-fit, a dovetail). The strongest and most reusable is usually a screw into a metal insert. Pick by asking three questions: how many times will it be opened, how big is the load, and in which direction does the load act relative to the layers.

JointReusableStrengthEasy to printHardwareBest for Snap-fit●●●○●●○○●●●○nonelids, clips Press / friction fit●●○○●●○○●●○○pin / dowelalignment Dovetail / slide●●●●●●○○●●●○nonedrawers, rails Screw + heat-set insert●●●●●●●●●●●○insert + screwservice panels Bolt + nut trap●●●●●●●○●●●○bolt + nutstructural Magnet●●●●●○○○●●○○magnetsdoors, mounts Glue / solvent weld○○○○●●●○●●●●adhesivesplit models ●●●● = best. Ratings are relative for a typical FDM part in PETG; they are guidance, not test data.
Figure 1. A quick map of joint choices. Start from the top (no hardware) and move down only when the load or the number of cycles demands it.
Rule of thumb

If it will be opened more than about five times, do not let plastic carry the thread or the latch alone. Use metal: an insert, a nut or a steel pin. If it will be opened once, print the latch and glue the rest.

🔧 Snap-fits

A snap-fit stores elastic energy in a flexing arm, lets a hook ride over an undercut and then relaxes behind it. Done well, it replaces screws. Done badly, it breaks the first time you use it, because plastic that is bent beyond its elastic strain limit cracks, and printed parts have lower limits than the datasheet suggests (layer lines act as built-in notches). Three families matter: cantilever, annular and torsional.

Cantilever snap-fit: the beam math

A cantilever snap is a beam fixed at one end with a hook on the other. For a beam of constant rectangular section, length L, thickness h (in the bending direction) and width b, pushed aside by a deflection y (the undercut depth):

εmax = 1.5 · h · y / L²   (strain at the root, as a fraction; ×100 for %)
P = E · b · h² · ε / (6 · L)   (force needed to deflect the tip by y)

Two things stand out. Strain grows with h and y but falls with the square of L: lengthening the arm by 50 % cuts strain by more than half. And force grows with h², so a thin, long arm is both gentle and safe.

L (length) y(undercut) h = beam thickness Wall (fixed end) with a root fillet of at least 0.5·h hook head ramp: lead-in Constant-section beam ε = 1.5 · h · y / L² P = E · b · h² · ε / (6L) Example (PLA, limit ε ≈ 0.8 %): h 1.6, L 18, y 1.0 mm ε = 1.5·1.6·1.0 / 324 = 0.74 % ✔ Same arm with L = 12 mm: ε = 1.67 % ✘ for PLA, ok for PETG Orange dashes = deflected position.
Figure 2. Cantilever snap-fit anatomy and the two formulas you need. Dimensions are in mm.

Strain limits by material

The permissible strain is the number that decides whether the design works. The values below are conservative design numbers for printed parts with layers running along the beam, not datasheet elongation. They are indicative: test one prototype before you commit to a design.

MaterialOne-off assembly (ε max)Repeated use (ε max)Comment
PLA0.8–1.0 %0.4 %Stiff and brittle; long, thin arms only. Fatigues quickly.
PETG2.0 %1.0 %The best everyday snap-fit material.
ABS / ASA1.8 %0.9 %Good if layer adhesion is good (warm chamber).
PC2.5 %1.2 %Tough but notch-sensitive; use big fillets.
Nylon (PA, dry)3.0–4.0 %1.5–2.0 %Excellent fatigue; absorbs moisture and softens.
PP4.0 %2.0 %Great for hinges and latches; difficult to print.
CF/GF-filled0.5–1.0 %0.3–0.5 %Stiffer, strain-limited: needs longer arms than unfilled.
TPU 95A5–8 %3–5 %Behaves like a spring; a snap arm may be unnecessary.
Print orientation decides everything

A snap arm must be printed so that the tensile stress runs along the extrusion lines, not across layers. A tall hook standing on its tip, bending sideways, will peel apart at a layer line at a fraction of the strain in the table.

Good: layers run along the arm push Tension acts along each layer: continuous plastic. Bad: arm stands on its tip push Bending pulls across layers: cracks at a layer line.
Figure 3. The same arm, two orientations. If the snap must stand upright, make it 2–3 times thicker or choose a different joint.

Make the arm better: taper and fillet

Strain peaks at the root of the arm. Two cheap changes lower it dramatically. Taper the thickness from h at the root to h/2 at the tip: strain follows ε ≈ 0.92 · h · y / L², which allows about 64 % more deflection for the same peak strain. And add a root fillet of at least 0.5 × h (1 mm minimum) so the stress is not concentrated in a sharp corner. Many failed snaps broke at a 90° corner at the root, not in the middle of the arm.

Constant ε = 1.5·h·y / L²reference (100 %)sharp root: stress riser Tapered to h/2 ε = 0.92·h·y / L²≈ 61 % of the strainbest material use Constant + root fillet fillet r ≥ 0.5·hpeak stress down 20–30 %easiest to model
Figure 4. Three ways to shape a snap arm. Combine taper and fillet for the longest life.

Hook geometry: how the angles set force

The hook has two faces. The lead-in (insertion) ramp sets how hard it is to push in; the return face sets how hard it is to pull out. A ramp at 30°–45° from the motion direction lets the part snap in with moderate force. A return face at 90° is a permanent lock; at 45°–60° it releases when you pull. Keep the undercut y at 0.5–1.2 mm and the hook head at least 1.6 mm (four lines) wide, or the tip will print as a fuzzy sliver.

Return face angleBehaviorUse
90° (flat)Permanent, breaks before it releasesSingle-use closures, boxes you never reopen
60–75°Releases with a firm pullBattery doors, rarely opened lids
45°Releases easily; may pop loose under vibrationFrequently opened lids, clips
30°Friction catch onlyLight detent, positioning

Annular snap-fit

An annular snap-fit is a ring that stretches over a bead: bottle caps, pen caps, round lids. The strain is the hoop (circumferential) strain: ε ≈ y / r, where y is the radial undercut and r the radius of the bead. A 20 mm diameter bead (r = 10 mm) with y = 0.2 mm gives 2 %: borderline for PETG, impossible for PLA. A ring is much stiffer than a beam, so cut 4–6 slits through the wall to turn it into separate cantilevers and then use the cantilever formula.

bead undercut y Lip locks under the bead Hoop strain in a ring ε ≈ y / r r = 10 mm, y = 0.2 mm → ε = 2 % PETG ok · PLA cracks · PA ok • Slit the ring (4–6 slits, 1 mm wide) to relieve hoop stress • Bead height y = 0.3–0.6 mm, 45° lead-in on the bead • Print with the axis vertical: layers run around the ring • Add 0.2–0.3 mm radial clearance everywhere else
Figure 5. A bead-and-lip annular snap in section. Layers run around the ring when the axis is vertical, which is the strong direction for hoop strain.

Torsional snap-fit

In a torsional snap the hook sits on a lever, and a thin bar acts as a torsion spring when you press the lever. It fits compact spaces where a long beam will not. For a thin rectangular bar of length L and thickness t twisted by an angle θ (radians), the maximum shear strain is roughly γ ≈ θ · t / L. Use shear-strain limits about 1.2–1.5 × the tension values above as a first guess.

Torsion bar: t = 1.2, L = 22 mm press θ = 12° = 0.21 rad → γ = 0.21 · 1.2 / 22 = 1.1 % fine for PETG or PA, too much for PLA Design notes • Bar thickness 1.0–1.6 mm (2–4 lines) • Bar length 15–30 mm; longer = softer • Print the bar flat so layers run along its length • Add a stop so the lever cannot over-rotate • Prefer square (not round) bar sections • Shear limit ≈ 1.2–1.5 × tension limit
Figure 6. A torsional snap stores energy in a twisting bar, saving the length a cantilever needs.

🚀 Living hinges

A living hinge is a thin web of material that bends repeatedly. In injection-molded polypropylene it can flex a million times; in printed plastic the story is more modest. PP and TPU are excellent, PETG survives tens to hundreds of cycles if designed carefully, and PLA breaks in a handful. Treat a printed living hinge as a limited-life part and consider a pin hinge for anything opened daily.

As printed (flat) web length 2 mm 0.5 mm thick Bent 90° web radius ≈ 2 mmstrain ≈ t / (2r) = 12 % Use a thickness of 1–1.5 lines (0.45–0.6 mm) and a web length of 2–3 mm for PETG. Print flat on the bed so the web lines run across the fold. TPU: 0.8–1.2 mm web. PLA: do not rely on it.
Figure 7. A 0.5 mm web bent through 90° with a 2 mm radius sees about 12 % outer-fiber strain, far above the elastic limit for most printed plastics, which is why the plastic yields once and then works as a cold-drawn hinge. Expect a short life.
MaterialWeb thicknessWeb lengthExpected life
PP0.4–0.5 mm1.5–3 mmThousands of cycles
PETG0.4–0.6 mm2–3 mm10–200 cycles
TPU 95A0.8–1.2 mm3–5 mmEffectively unlimited
Nylon (dry)0.4–0.6 mm2–3 mm100–1,000 cycles
PLA––Few; do not use

🔧 Press fits, dovetails, finger joints and puzzles

Joints that rely on geometry alone are the most elegant and the most sensitive to tolerance. All gaps below are per face, for a 0.4 mm nozzle, and assume you read the clearance table first.

Dovetail60–75° flanksgap 0.2–0.3 per faceslide length ≥ 15 mm Finger / box jointfinger 4–8 mm widegap 0.1–0.2 per sideglue for strength Tongue & groovetongue ≈ ⅓ thickness (≥ 1.2)depth 3–5, gap 0.15–0.25self-aligns panels Puzzle knobneck ≥ 3 mmknob ≈ 1.5 × neckgap 0.15–0.25 All four print flat; the loaded direction should never pull layers apart (see Strength & orientation).
Figure 8. Shape-locked joints. Dovetails and puzzle knobs lock in two axes; finger joints give large glue area; tongue and groove aligns thin panels.
JointKey numbers (0.4 mm nozzle)Watch out
Press-fit pinPin Ø 0–0.1 larger than hole (diametral); 0.5 mm lead-in chamfer; depth ≥ 2 × ØCreep: the grip loosens over weeks in PLA/PETG
DovetailFlank angle 60–75°; clearance 0.2–0.3; add a 1–2° taper along the slide for a wedge-lockPrint with the slide axis along the layers
Finger jointFinger width 4–8 mm; clearance 0.1–0.2; ≥ 3 fingersCorner stress; fillet the finger roots 0.5 mm
Tongue & grooveTongue ⅓ wall thickness, ≥ 1.2; depth 3–5; clearance 0.15–0.25Thin tongues break; keep them ≥ 3 lines
Puzzle knobNeck ≥ 3; knob 1.5 × neck; clearance 0.15–0.25 per sideCorners need 1 mm fillets or they crack

🔧 Bolted joints: clearance holes, counterbores and nut traps

A bolt and nut clamp two parts with a force that plastic cannot match, but plastic must carry the clamping load without crushing. Use a washer or a counterbore with a flat floor under the head, keep the clamp length at least 3 mm of solid plastic, and never overtighten: stop when the surfaces touch. Tightening torque on printed parts is often finger-tight plus a quarter turn.

Counterbore (section) head Ø + 0.5 k + 0.3 Clearance hole Ø = bolt Ø + 0.4 Floor flat; head stays below the surface Nut trap (plan) AF + 0.2–0.3 Hex across corners = AF × 1.155 Side slot lets the nut slide in Nut trap rules • Pocket depth = nut m + 0.3 • 0.2–0.3 mm clearance on AF • Open the pocket to the side (slot) or from the bottom • Top-loaded pocket: pause at the layer, drop the nut in • Walls around the pocket ≥ 3 perimeters (1.35 mm) • Tighten along Z: nut pulls layers together, not apart
Figure 9. A counterbore hides the head; a hexagonal pocket with a slot holds the nut while you tighten. Hexagon corners print rounded, so give 0.2–0.3 mm of clearance on across-flats.
ScrewClearance hole ØSocket head Ø × kCounterbore Ø × depthNut AF × mNut pocket AF × depth
M22.43.8 × 2.04.4 × 2.34.0 × 1.64.2 × 1.9
M2.52.94.5 × 2.55.0 × 2.85.0 × 2.05.2 × 2.3
M33.45.5 × 3.06.0 × 3.35.5 × 2.45.8 × 2.7
M44.57.0 × 4.07.6 × 4.37.0 × 3.27.3 × 3.5
M55.58.5 × 5.09.2 × 5.38.0 × 4.08.3 × 4.3
M66.610.0 × 6.010.8 × 6.310.0 × 5.010.3 × 5.3
M88.613.0 × 8.014.0 × 8.313.0 × 6.513.3 × 6.8

All in mm; dimensions for metric socket-head cap screws and standard (ISO 4032) nuts. Hole sizes add the slip-fit allowance of the printed hole; for a horizontal hole, make it a teardrop (hole shapes).

🚀 Heat-set inserts

A brass heat-set insert is melted into a printed pocket with a soldering iron. The plastic flows into the knurls, solidifies, and you have a metal thread that survives hundreds of screw cycles and pulls out at hundreds of newtons. It is the best way to put a thread in a printed part. The recipe is a hole slightly smaller than the insert, a relief pocket underneath for displaced plastic, and a boss wide enough to take the pressure.

boss Ø ≥ 2 × insert Ø pocket depth= insert + 1 hole = OD − 0.5 relief Installation 1. Iron with insert tip at 200–230 °C (PLA, PETG),230–260 °C (ABS, ASA, PA) 2. Rest the insert on the hole, let the heat soak in 3. Press straight and slowly; stop when flush 4. Do not push further; remove the iron, hold still 10 s 5. Test the thread with a screw, not a drill Insert pulls along Z? Layers parallel to the pull are weak: add a wall of ≥ 4 perimeters or put the insert in a vertical boss.
Figure 10. Heat-set insert pocket: a hole smaller than the insert, a relief below for displaced plastic, a chamfer at the mouth, and a boss at least twice the insert diameter.
ThreadTypical insert OD × lengthPocket hole ØPocket depthBoss Ø (min)
M23.5 × 3–43.25.07
M2.54.0 × 43.6–3.85.58
M34.6 × 5–64.0–4.27.09
M46.0 × 6–85.4–5.69.012
M57.0 × 8–106.4–6.611.014
M68.5 × 10–127.8–8.013.017
M811 × 12–1410.2–10.415.022

Mm. Insert dimensions vary between manufacturers: always check the datasheet and print a test pocket with two different diameters. Use the smaller hole for PLA and the larger for PETG/ABS if the insert barely fits.

🔧 Self-tapping screws and screw bosses

A screw can cut its own thread in a plain pilot hole in printed plastic. It is quick but wears out in 3–5 cycles. Choose it for single-use or low-load closures. The boss that carries the screw must be strong enough not to split: a pilot hole of about 0.8 × the screw diameter, a boss outer diameter of 2.5–3 × the screw, a thread engagement of at least 2 × the screw diameter, and gussets (ribs) to the main wall.

boss Ø 2.5–3 × d engagement≥ 2 × d Gussets 60–100 % of wall thickness; fillet 1 mm to the base Screw boss checklist • Pilot Ø ≈ 0.8 × screw: M2 1.7 · M2.5 2.1M3 2.5–2.6 · M4 3.3–3.4 mm • Boss wall ≥ 1.6 mm (4 lines) around the pilot • 2–4 gussets, one per 90–120° of boss • Do not connect the boss to a thin outer wallwithout a rib: it sinks or pops out • Chamfer the pilot entry 0.5 mm • Use a thread-forming screw, not a bolt
Figure 11. A screw boss with gussets. The boss is a column, so print it vertically and keep the pilot hole in the same direction as the screw.

🔧 Threads: printed, modeled or tapped

There are three honest ways to get a thread in a printed part, and they differ by two orders of magnitude in durability. Detailed clearances for printed threads are on the tolerance page; here is how to choose.

Printed thread pitch ≥ 2 mm, Ø ≥ 12 mm3–10 cycles; best as a capno extra hardware Tapped in plastic M3 into Ø 2.7–2.8 mm hole5–20 cycles; cut with a hand taponly for low loads Heat-set insert metal thread in plastic100+ cycles; hundreds of Nneeds inserts and a hot iron
Figure 12. Three kinds of thread. The metal insert is by far the most durable; modeled threads below M12 are usually a waste of effort.
Big threads, big pitch

A printed thread needs about 3–4 layers per thread flank to be strong. A pitch of 2 mm with a 0.2 mm layer gives about 10 layers per pitch: good. Fine M3 (0.5 mm pitch) cannot be modeled with a 0.4 mm nozzle: the crests merge into a ridge. Use real hardware for small sizes.

🔧 Magnets

Disc magnets (neodymium) give a hinge-free closure, a modular mounting system or a tool holder. The design problem is the pocket: it must hold the magnet against the pull, keep the magnet close to the contact face and not let it flip. Make the pocket 0.1–0.2 mm larger in diameter than the magnet for a glue fit (or 0.05–0.1 for a press fit in PETG), 0.1–0.2 mm deeper than the magnet thickness, and leave a front skin of 0.4–0.6 mm (two to three layers). Every extra 0.5 mm of plastic between magnet faces cuts holding force by roughly a quarter.

skin 0.4–0.6 mm Pocket opens at the back or is paused and capped Add a dab of CA or epoxy NS Mark polarity with a notch,a key or a shaped pocket soa magnet cannot be flipped. Safety • Keep away from pacemakers• Swallowing hazard: seal pockets• Pinch hazard when pairs snap• Neodymium weakens above ~80 °C• Brittle: they chip when slammed• Never grind or drill them
Figure 13. Magnet pocket with a thin skin and a polarity key. Insert the magnet while the print is paused, then cover it with 2–3 layers.
Magnet (Ø × t)Pocket Ø (glue fit)Pocket Ø (press fit)Pocket depthBoss/wall around pocket
5 × 25.25.12.2≥ 1.2
6 × 36.26.13.2≥ 1.2
8 × 38.28.13.2≥ 1.6
10 × 310.210.13.2≥ 1.6
12 × 312.212.13.2≥ 2.0

🔧 Pins and hinges

A pin hinge is the workhorse of printed mechanisms. The pin can be a piece of 1.75 mm filament (cheap, in a 1.9–2.0 mm hole), a nail or steel rod, or a printed pin. The rules: a slip fit in the knuckles that rotate and a snug fit in the knuckles that must hold the pin, 0.3–0.5 mm gap between the knuckles so they never fuse, knuckles at least 3 × the pin diameter long, and a retaining feature at each end (a mushroomed filament end, a cap or a cotter pin).

Part APart B knuckle gap 0.4 A: snug hole (pin + 0.1) · B: slip hole (pin + 0.3) Pin options • 1.75 mm filament in Ø 1.9–2.0: free, flexible,flatten the end with a hot iron as a rivet head • Steel rod / nail: stiff; use for load • Printed pin: print standing so layers circlethe pin (strong in bending) • Snap-in pin: two small cone detents • Horizontal holes: use teardrops, not circles
Figure 14. A three-knuckle hinge: the middle knuckle belongs to one part and the outer two to the other, which spreads the load across the pin.

A print-in-place joint is printed fully assembled: the hinge, ball joint or chain link moves right off the bed. The key is a gap that survives printing without fusing: 0.3–0.5 mm in the horizontal plane, and in the vertical direction at least two layers (0.4 mm for 0.2 mm layers). Surfaces facing downward over the gap must be 45° chamfers so that no support is needed inside the mechanism.

gap 0.4 Pin Ø 8 in ring Ø 8.8 (≈ 0.4 per side) Print-in-place rules • Horizontal gap 0.3–0.5 mm; vertical gap ≥ 0.4 mm • Use 45° cone or chamfer faces for any gap that faces down • First layers fuse: widen the bottom gap by 0.2 mm or chamfer it • Calibrate flow and use a cooler nozzle: oozing bridges the gap • Keep outer-wall order consistent and avoid ironing near gaps • Free the joint with a twist or a thin knife along the gap • Avoid brims that cross the gap • Print a one-link test before the full model
Figure 15. Plan view of a print-in-place pin. Both the gap width and the printed layer height decide whether the joint frees.

🔧 Adhesive joints and glue channels

Glue is the best way to assemble models that were split to fit the bed. Think of the glue line as a part of the joint: give it surface area, a controlled gap and a place for excess to go. Cyanoacrylate (CA, superglue) gives fast bonds on PLA and PETG, two-part epoxy fills gaps and bonds nearly everything, and solvent welding works on ABS and ASA (acetone), where it melts the surfaces together and gives close to parent-material strength. Sand surfaces to 120–220 grit first and wipe with isopropyl alcohol.

glue gap 0.1–0.2 Channels 1 × 1 mm hold glue and let air escape Scarf joint: cut at 10–20° to the axisGlue area ≈ 4–6 × the cross-section Best for tubes and long rods CureCA: secondsEpoxy: 5 min–24 hClamp, no gapsUse gloves, ventilate
Figure 16. A lap joint with glue reservoirs and a scarf joint. A flat butt joint is the weakest option: avoid it unless you add alignment features.

🔧 Ribs, gussets and fillets

Ribs stiffen thin walls cheaply; gussets support a corner; fillets spread stress. For FDM the rules are simple: rib thickness 0.9–1.8 mm (2–4 lines, at most the wall it sits on), rib height at most 4–5 × its thickness before it buckles or wobbles, and an inside corner fillet of at least 1 mm (3 mm in loaded corners). Orient ribs along the load, and remember that a rib in the XY plane is strong in the layer plane but weak if it is pulled in Z.

Rib thickness 0.9–1.8; height ≤ 4–5 ×rib spacing ≥ 3 × wall Gusset triangle ≥ 45° steep, leg ≥ 10 mmcuts bending stress by 50–70 % Fillet r ≥ 1 mm (loaded: 3+ mm)no sharp inside corners
Figure 17. Three ways to stiffen an L-shaped part. A gusset costs a little plastic and a fillet costs nothing.

🔧 Splitting large parts with alignment features

When a part is larger than the bed (256 × 256 mm on the X2D; much smaller on many printers), cut it into pieces that print flat, then assemble. Cut at places where the seam is hidden (an edge, a groove), keep each piece's cut face flat on the bed, and give every joint an alignment feature: pegs (Ø 4–6 mm, length 6–8 mm, 0.2 mm clearance), a tongue and groove along the seam, or a dovetail key across it. Glue over the full face; the alignment features carry shear, the glue carries tension.

Part 1 (cut face on the bed)Part 2 Peg: Ø 4–6, length 6–8Socket: peg + 0.2, depth + 0.5 Splitting tips • Split along existing edges or grooves • Use 2+ pegs, not in line with the load • Avoid long straight seams on visible faces • Add 0.1–0.2 mm gap between the faces for glue • Give pegs a 0.5 mm lead-in chamfer • Print a one-piece test of the seam first • Sand and prime seams before painting
Figure 18. A split part with pegs and sockets. Dashed line: seam. Every plane cut becomes a flat face on the bed with no supports required.

🔧 Hardware pockets and bearings

A pocket for a nut, magnet, bearing or electronic part follows the same rules: opening size = part + clearance, depth = part + 0.1–0.2 mm, a retainer (lip, cover or glue), and walls of at least 1.2 mm around. A standard ball bearing needs a round pocket slightly smaller than the outer race for a press fit, and a step at the bottom to carry axial load. For vertical bores a bridge-free design (hexagonal or chamfered ceiling) avoids supports inside.

Ø 22.1–22.3 (press 22.0) 7.2 Shoulder 1 mm; shaft hole Ø 8.4Retainer: 0.4 mm lip or cover Common bearings: pocket sizes Bearing ID×OD×W pocket Ø × depth 623 3×10×4 10.1 × 4.2 624 4×13×5 13.1 × 5.2 625 5×16×5 16.1 × 5.2 608 8×22×7 22.1 × 7.2 6000 10×26×8 26.1 × 8.2 Adjust ±0.1 to your printer. Warm PETG/ABSrelaxes the press; use CA glue for permanent. Print the bore vertically for round, exact pockets.
Figure 19. A 608 skateboard bearing in a press-fit pocket with a lower shoulder. Dimensions in mm for a 0.4 mm nozzle.

🔧 Gears: involute, backlash and herringbone

Printed gears work well for light loads, if you choose a large enough module (m = pitch diameter ÷ tooth count). With a 0.4 mm nozzle use m ≥ 1.5 (preferably 2): at m = 2 a tooth is about 3.1 mm thick at the pitch line, or seven lines. Use a 20° pressure angle with the involute profile (this is what every gear library gives you) and at least 17 teeth on the smaller gear to avoid undercut. Mesh them at a center distance of a = m·(z₁ + z₂)/2 + 0.1–0.2 mm, where the added term is the backlash that stops the gears binding when printed teeth are slightly fat.

pitch line · module 2 · pitch 6.28 mm tooth height 4.5 · backlash 0.1–0.2 (exaggerated) Printed gear checklist • Module 1.5–2 for 0.4 nozzle; face width 4–6 × m • Pressure angle 20°; ≥ 17 teeth (or profile shift) • Center distance = m(z₁+z₂)/2 + 0.1–0.2 mm • Print the gear flat: teeth then bend along layers • Herringbone: two opposed helixes cancel axial force,helix angle 20–30°, no gap in the middle for easy print • Hub: 3 mm minimum wall; use a set screw or D-flat • PETG, PA or POM-like filaments run quieter than PLA
Figure 20. Teeth of two meshing gears, shown unwrapped as racks. Each flank must clear the opposite one by the backlash allowance.

🔧 Cable management

A cable clip needs an opening narrower than the cable so it stays, but wide enough that the clip can stretch open without breaking. Size the hole 0.4–0.6 mm over the cable diameter, the opening at 70–80 % of the diameter and the wall at 1.6–2.0 mm. Print the clip lying flat so the layers wrap around the cable: each flex then stretches the layers instead of peeling them. For bundles, a slot for a hook-and-loop strap or a zip tie (slot 4 × 1.6 mm for a 2.5 mm tie) is more flexible than a fixed clamp.

opening 0.7–0.8 × Ø Hole = cable Ø + 0.5Wall 1.6–2.0 mmFlat on the bed Tie slot 4 × 1.6 mmSlot spacing ≥ 6 mm Cable rules • Fillet every sharp edge 1 mm (no cable damage) • Screw hole Ø 3.4 plus a counterbore for M3 • Adhesive foam pad: flat base ≥ 15 × 15 mm • Hot cables: use ASA or PC, not PLA • Keep a 3 mm minimum bend radius for thin cables;10× diameter for coax and power
Figure 21. A C-clip and a zip-tie plate: the clip opening is narrower than the cable; the plate takes any tie.

🔧 Standoffs and electronics mounting

A standoff lifts a circuit board off the floor of an enclosure. Use a post with a locating pin (pin Ø = board hole − 0.2 mm, height equal to the board thickness 1.6 mm plus 0.5 mm) or a screw boss with an insert (see above). Height is set by the tallest solder joint under the board plus 1–2 mm; a typical value is 4–6 mm. Make the standoff base fillet 1 mm and its diameter at least 2 × the pin or screw (M2.5 → 6 mm).

4–6 mm PCB 1.6 mm · pin Ø = hole − 0.2 · base fillet 1 mm Standoff rules • Locate with pins or M2.5/M3 inserts • 4 corner posts + 1 center support if long • Keep clear of the largest component • Add cable and connector cut-outs at +0.5 • Insulating plastic only: do not use metalfilaments under live boards
Figure 22. A board on printed standoffs with locating pins. The same idea becomes a screw boss when the board is screwed down.

Key takeaways

Next: Strength & orientation explains the layer-direction logic behind these rules, and Design patterns puts the joints to work in complete designs.